A515 Gr.65 Boiler Quality Plate Materials

A515 Gr.65 Boiler Quality Plate Materials

ASTM A515 Gr 60 Steel Plates is a carbon-silicon steel produced according to the American Standard ASTM A515/A515M. It has high strength and toughness, good weldability, impact resistance, and fatigue resistance. These plates are mainly used in pressure vessels at moderate and lower temperatures.
Mô tả
Thông số kỹ thuật

A515 Gr.65 Boiler Quality Plate Materials


ASTM A515 Gr.65 carbon steel plates are mainly used for medium and high temperature pressure vessels. They are widely used in boiler manufacturing in industries such as shipbuilding, petrochemicals, and manufacturing.

 

GNEE Group is a professional ASTM A515 Gr.65 boiler steel plate stockist and supplier. We can supply different types and grades of ASTM A515 products. If you have any needs for ASTM A515 Gr.65 vessel steel plate, please feel free to contact us.

 

 
A515 gr.65 Boiler Quality Steel Plates chemical composition

 

0.28 %

max.|for thickness 5-25 mm

 

0.31 %

max.|for thickness 25-50 mm

 

0.33 %

max.|for thickness 50-80 mm

0.9 %

max.|for thickness 5-80 mm

0.025 %

max.|for thickness 5-80 mm

0.15 - 0.4 %

for thickness 5-80 mm

0.025 %

max.|for thickness 5-80 mm

 

 
a515 gr.65 Hot rolled boiler steel plates mechanical property

 

19 %

min.|for thickness 5-80 mm|A8|Transverse

 

23 %

min.|for thickness 5-80 mm|A2|Transverse

450 - 585 MPa

for thickness 5-80 mm|Transverse

240 MPa

min.|for thickness 5-80 mm|Transverse

 

 
 
China steel boiler plate Suppliers
China Boiler Plate Steel Manufacturers
China pressure vessel plate Distributors
 

 

China pressure vessel steel manufacturer

 

 
China pressure vessel steel plate Manufacturers
China pressure vessel quality steel Manufacturers
40
China pressure vessel steel manufacturer
China boiler steel plate Manufacturers
China steel boiler plate Distributors
 
China boiler quality plates Suppliers
China pvq plate Suppliers
China vessel plate Manufacturers
China boiler plate Manufacturers
China pressure vessel steel Distributors
China carbon steel pressure vessel Manufacturers

We have professional online service personnel. If you have any questions about A515 Gr.65 Boiler Quality Plate Materials, please send us an inquiry and we will reply to you within one working day.

 

Chú phổ biến: a515 gr.65 boiler quality plate materials, China a515 gr.65 boiler quality plate materials manufacturers, suppliers, factory